Flat braided Wire Sling
Product Parameters

|
|
|
|
|
|
|
|
| Type | Min. bending diameter D | Straight WLL Ton | Choke WLL Ton | Basket WLL Ton | Basket 0°-45° WLL Ton | Basket 45°-60° WLL Ton | |
| mm | |||||||
| ZH09500 | 115 | 0.95 | 0.76 | 1.9 | 1.33 | 0.95 | |
| ZH16000 | 150 | 1.6 | 1.2 | 3.2 | 2.2 | 1.6 | |
| ZH25000 | 190 | 2.5 | 2 | 5 | 3.5 | 2.5 | |
| ZH32000 | 230 | 3.2 | 2.5 | 6.4 | 4.4 | 3.2 | |
| ZH48000 | 265 | 4.8 | 3.8 | 9.6 | 6.7 | 4.8 | |
| ZH58000 | 300 | 5.8 | 4.6 | 11.6 | 8.1 | 5.8 | |
| ZH80000 | 400 | 8 | 6.4 | 16 | 11.2 | 8.0 | |
| ZH11000 | 450 | 11 | 8.8 | 22 | 15.4 | 11 | |
| Factor(K) | 1 | 0.8 | 2 | 1.4 | 1 |
Product Detail
1. Drive the short end of the wire rope to the end of the inspection hole. See fiqure. Check before swaging!
Note: The ends of the wire rope shall not have any tape or secure servings that could be swaged inside the ferrule.
2. Place the ferrule with the inspection holeover the pin. The position of the ferrule is automaticallysecured in the press die.
3. Verify that the tail ends of the wire ropes isvisible in the inspection hole after swaging.4. Remove the flash material.
5. Check the diameter after swaging according to this specification.
NOTE!
Replace tap when wom or damaged.
Do not swage without tap or blind tap.
Contact the manufacturer if it cannot be removed.
Features:
.Flat braided wire sling for advanced lifting in all industries.
.Flat braided Wire Slings are manufactured with aluminium conical ferrule
.Lots are break tested in the factory before delivery.
.Each Sling is marked with serial number that links to the test certificate with full traceability to raw material.
.Fatigue tested according to EN13411-3.
Steel Wire Rope: Galvanized 6x19M-WSC 1960N/ mm² acc.to EN12385-4
Ferrule: Conical aluminium ferrule with inspection hole acc.to EN13411-3
Working temperature: -40°C up to +150°C.
Standard: Machinery directive 2006/42/EC
Safety factor: 5:1